Shotcrete Practices at the Henderson Mine

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shotcrete Practices at the Henderson Mine

Author(s): Robert C. Jones

Publication: Symposium Paper

Volume: 45

Issue:

Appears on pages(s): 50-56

Keywords:

DOI: 10.14359/17934

Date: 1/1/1974

Abstract:
The Henderson Mine is being developed by American Metal Climax. It is located about 50 miles west of Denver, Colorado, adjacent to the Continental Divide. The mine site is in a narrow canyon at an elevation of 10,400 feet above sea level.