E2-00: Reinforcement for Concrete - Materials and Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: E2-00: Reinforcement for Concrete - Materials and Applications

Author(s): ACI Committee E701

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords:

DOI:

Date: 1/1/2000

Abstract:
This publication provides an introduction to commonly used materials for reinforcement of concrete, and describes the basic properties and uses of these materials. Topics covered include plain, reinforced, and prestressed concrete; reinforcing and prestressing materials; corrosion-resistant reinforcement; and storage and handling. NOTE: Free downloadable version of this document is now available from the " Technical > Concrete Knowledge Center > Consensus Documents > Materials for Concrete Construction" section of the ACI Website Home Page.