Pumping Fibrous Concrete for Spillway Test

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pumping Fibrous Concrete for Spillway Test

Author(s): Richard A. Kaden

Publication: Symposium Paper

Volume: 44

Issue:

Appears on pages(s): 497-510

Keywords: compressive strength; concrete construction; fiber reinforced concretes; flexural strength; freeze-thaw durability; metal fibers; modulus of elasticity; placing; pumped concretes; quality control; repairs; sillways; splitting tensile strength

DOI: 10.14359/17912

Date: 1/1/1974

Abstract:
This report describes the use of steel fiber reinforced concrete as a construction material for high velocity water passages, specifically the wearing surfaces of flip lips on high velocity spillways. . .The results from both field and laboratory tests performed for acceptance, evaluation, and quality control are reported.