Pavement and Bridge Deck Overlays with Steel Fibrous Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pavement and Bridge Deck Overlays with Steel Fibrous Concrete

Author(s): David R. Lankard and Alvin J. Walker

Publication: Symposium Paper

Volume: 44

Issue:

Appears on pages(s): 375-392

Keywords: bonding; bridge decks; concretes; fiber reinforced; concretes; highways; joints (junctions); metal fibers; mix proportioning; pavements; placing; resurfacing

DOI: 10.14359/17906

Date: 1/1/1974

Abstract:
Field experiments designed to evaluate the suitability and effectiveness of steel fibrous concrete as on overlay material for bridge decks, highway pavements, and airfield pavements have been carried out and others are planned. Although it will require many years before a complete assessment can be made of the performance of the experimental fibrous concrete overlays, the initial experiences and results have been encouraging.