Title: On the Properties and Behavior of High Early Strength Lightweight Polymer Impregnated Resistant Glass Fibers

Author(s): M. Gunasekaran, Y. Ichikawa, and A.B. Dunlap

Publication: Symposium Paper

Volume: 44

Issue:

Appears on pages(s): 265-286

Keywords: compressive strength; fiber reinforced concretes; fibers; flexural strength; fly ash; glass fibers; high early strength cements; humidity; impregnating; lightweight aggregate concretes; lightweight aggregates; polymer concrete; research; shrinkage

DOI: 10.14359/17899

Date: 1/1/1974

Abstract:
Some of the principal structural properties of lightweight, sintered fly-ash aggregate concrete made with Regulated Set Cement and reinforced with alkali-resistant glass fibers are presented.