Title: The Effect of Steel Fibers on the Compressive Strength of Concrete

Author(s): Gilbert R. Williamson

Publication: Symposium Paper

Volume: 44

Issue:

Appears on pages(s): 195-208

Keywords: aggregates; compressive strength; concrete durability; cracking (fracturing); fiber reinforced concretes; metal fibers; mix proportioning; modulus of elasticity; mortars (material); poisson ratio; research

DOI: 10.14359/17894

Date: 1/1/1974

Abstract:
The effect of steel fibers on the static compression strength of concrete and mortar was studied. . .Values for Young's modulus and Poisson's ratio for the various fiber percentages are also given.