Title: C-18: Shotcrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 76

Keywords:

DOI:

Date: 1/1/1992

Abstract:

Note: C-18 is No Longer Available.

This compilation of "Concrete International" magazine articles on shotcrete also includes Letters to the Editor on the subject. A sampling of the subject area includes steel fiber-reinforced shotcrete, high-early-strength west-process shotcrete, use of silica fume in shotcrete, and use of shotcrete for new construction and repair. Several articles deal with durability of shotcrete.