Using the Recommended Practice for Selecting Proportions for Structural Lightweight Concrete (ACI 211.2-69)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Using the Recommended Practice for Selecting Proportions for Structural Lightweight Concrete (ACI 211.2-69)

Author(s): William W. Hotaling, Jr.

Publication: Symposium Paper

Volume: 46

Issue:

Appears on pages(s): 209-220

Keywords: absorption; aggregate gradation; air entrainment; cement content; coarse aggregates; density (mass/volume); fine aggregates; fineness modulus; lightweight aggregates concretes; lightweight aggregates; mix proportioning; moisture content; quality control

DOI: 10.14359/17877

Date: 1/1/1974

Abstract:
The Recommended Practice for Selecting Proportions for Structural Lightweight Concrete (ACI 211.2-69) presents methods for designing structural lightweight concrete mixes, emphasizing their adjustment by employing a specific gravity factor. This in turn enables calculation of effective displaced volumes for the lightweight aggregate fractions in the mixture. Developed via a pycnometer, these factors are presented as a continuous function for a range of aggregate moisture contents. Also included in the Standard are adjustment guides as well as field control pointers.