A New High Early Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A New High Early Strength Concrete

Author(s): Robert O. Russell

Publication: Symposium Paper

Volume: 51

Issue:

Appears on pages(s): 269-278

Keywords: aggregates; autoclaving; bonding; compressive strength; concrete pavements; cold weather construction; deterioration; freeze-thaw durability; high early strength cements; mix proportioning; modulus of elasticity; Poisson's ratio; porosity; research; tests

DOI: 10.14359/17819

Date: 1/1/1975

Abstract:
A fast setting concrete product has been developed at Republic Steel's Research Center, Cleveland. This development was derived as an offshoot of refractory bonding programs oriented toward chemically bonded refractories. The bonding concept of this novel concrete is based on an acid-base reaction.