Title: First Progress Report on Concrete Experimental Test Sections in Brazos County, Texas

Author(s): J.L. Davis, W.B. Ledbetter, and A.H. Meyer

Publication: Symposium Paper

Volume: 51

Issue:

Appears on pages(s): 211-230

Keywords: concrete construction; concrete pavements; continuously reinforced concrete; finishes; research; skid resistance; test roads; texture; wear

DOI: 10.14359/17816

Date: 1/1/1975

Abstract:
Seven experimental test sections of CRCP were constructed in order to quantify the relative effects of the surface textures. Preliminary conclusions are reached after the first year's observation and are stated throughout the rest of the synopsis.