Prestressed Concrete, a Natural For Highway and Airport Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prestressed Concrete, a Natural For Highway and Airport Pavements

Author(s): Bengt F. Friberg

Publication: Symposium Paper

Volume: 51

Issue:

Appears on pages(s): 197-210

Keywords: airports; concrete construction; concrete pavements; continously reinforced pavements; control joints; cracking (fracturing) dowels; flexural strength; friction; highways; performance tests; post-tensioning; prestressed concrete; prestressing; shrinkage

DOI: 10.14359/17815

Date: 1/1/1975

Abstract:
The paper gives the major characteristics of the prestressed highway pavements which have been built in the United States during 1971-73, together with reasons for their design features. . This paper suggests suitable criteria for design and construction of future highway pavement (prestressed) projects. This criteria is also applicable for airports.