Airfield Pavement Construction: Slip Form Paving Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Airfield Pavement Construction: Slip Form Paving Method

Author(s): Frazier Parker, Jr.

Publication: Symposium Paper

Volume: 51

Issue:

Appears on pages(s): 51-72

Keywords: airports; concrete construction; concrete pavements; construction equipment; construction; materials; cracking (fracturing); deflection; dowels; joints (junctions); keys and keyways; mix proportioning; modulus of elasticity; paying equipment

DOI: 10.14359/17809

Date: 1/1/1975

Abstract:
This paper presents the results of a study to evaluate the use of slip-form paving equipment for the construction of airfield pavements. Nine construction projects were observed and surface smoothness measurements were made on eight of the projects.