Title: An Investigation of the Properties of Polymer Concrete

Author(s): J. Douglas Burleson, Chalmers G. Long, Jr., Constantine D. Armeniades, and Nat W. Krahl

Publication: Symposium Paper

Volume: 58

Issue:

Appears on pages(s): 1-20

Keywords: aggregates; compressive strength; concretes; curing; fiber reinforced concretes; mix proportioning; modulus of elasticity; polyester resins; polymer concrete; stress-strain relationships; tensile strength

DOI: 10.14359/17804

Date: 1/1/1978

Abstract:
An investigation of various formulations of polymer and aggregate composites was undertaken in order to determine possible applications of these new materials in building construction.