Investigation of Concrete Impregnated with Sulfur at Atmospheric Pressure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Investigation of Concrete Impregnated with Sulfur at Atmospheric Pressure

Author(s): S.P. Shah, A.E. Naaman, and R.H. Smith

Publication: Symposium Paper

Volume: 58

Issue:

Appears on pages(s): 399-416

Keywords: compressive strength; concrete durability; concretes; ductility; elastic properties; fiber reinforced concretes; impregnating; polymerization; sulfur; temperature

DOI: 10.14359/17803

Date: 1/1/1978

Abstract:
The primary purpose of this investigation was to study the feasibility and effects of sulfur impregnation of concrete carried out at atmospheric pressure. The investigation had three parts: to study the effects of process technology parameters (mix proportions, time of curing, temperature of drying and time of immersion in molten sulfur bath), to analyze the effects of high temperature and temperature cycling on properties of impregnated concrete, and to explore the possiblility of improving strength and ductiliy of SIC by addition of steel fibers.