Title: Polymer Impregnation Used in Concrete Repairs of Cavitation/Erosion Damage

Author(s): Ernest K. Schrader, David W. Fowler, Richard A. Kaden, and Rodney J. Stebbins

Publication: Symposium Paper

Volume: 58

Issue:

Appears on pages(s): 225-248

Keywords: concrete dams; costs; dry pack mortar; fiber reinforced concretes; impregnating; patching; plastics, polymers and resins; repairs

DOI: 10.14359/17794

Date: 1/1/1978

Abstract:
This paper discusses the use of polymer impregnation in the repairs of concrete damaged by cavitation/erosion forces at a major dam.