Study of Commerical Development in Precast Polymer Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study of Commerical Development in Precast Polymer Concrete

Author(s): Richard C. Prusinski

Publication: Symposium Paper

Volume: 58

Issue:

Appears on pages(s): 75-102

Keywords: concrete construction; concrete panels; costs; economics; floors; glass fibers; insulation; polyester resins; polymer concrete; precast concrete; reinforcing materials; resin concrete

DOI: 10.14359/17786

Date: 1/1/1978

Abstract:
The author traces the development and the art of an idea from its conception through a step by step process which evolves into end products. These have had a direct positive economic impact on the construction industry over the last two decades. He gives evidence of an ever expanding market in the immediate future where contemporary needs can be fulfilled with contemporary materials.