Torsional Strength of Reinforced and Prestressed Concrete Beams-CEB Approach

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Torsional Strength of Reinforced and Prestressed Concrete Beams-CEB Approach

Author(s): Burno Thurlimann

Publication: Symposium Paper

Volume: 59

Issue:

Appears on pages(s): 117-144

Keywords: beams (supports); bending; prestressed concrete; reinforced concrete; shear properties; structural design; torsion

DOI: 10.14359/17768

Date: 1/1/1979

Abstract:
Besides a "Standard Method" derived from semi-empirical considerations for the new CEB model code proposes a "Refined Method" for the design of reinforced and prestressed conrete members subjected to torsion. It is compatible with the design method for bending and shear and combined cases of bending, shear and torsion.