Shear Strength of Reinforced and Prestressed Concrete-CEB Approach

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Reinforced and Prestressed Concrete-CEB Approach

Author(s): Burno Thurlimann

Publication: Symposium Paper

Volume: 59

Issue:

Appears on pages(s): 93-116

Keywords: beams (supports); bending; building codes; plasticity; prestressed concrete; reinforced concrete; shear strength; structural design; ultimate strength method; web reinforcement

DOI: 10.14359/17767

Date: 1/1/1979

Abstract:
Besides a "Standard Method" derived from semi-empirical considerations for the new CEB model code proposes a "Refined Method" for the design of reinforced and prestressed concrete members subjected to bending and shear. It is compatiable with the design method for torsion and combined cases of bending, shear and torsion.