Laboratory Evaluation of a Concrete Superplasticizing Admixture

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Laboratory Evaluation of a Concrete Superplasticizing Admixture

Author(s): P.K. Mukherjee and B. Chojnacki

Publication: Symposium Paper

Volume: 62

Issue:

Appears on pages(s): 245-262

Keywords: admixtures; air-entraining agents; air entrainment; compressive strength; concretes; density (mass/volume); drying shrinkage; flexural strength; freeze-thaw durability; fresh concretes; hardened concretes; laboratories; modulus of elasticity; plasticizers

DOI: 10.14359/17728

Date: 1/1/1979

Abstract:
A superplasticizing admixture of the sulphonated melamine formaldehyde condensate type was tested in the laboratory for its effect on concrete mixes with a nominal slump of 3 in. (75 mm) and 415 kg/m3, respectively). A total of nine mixes were prepared. All mixes contained an air entraining admixture.