High-Range Water-Reducing Admixtures; Effect on the Air-Void System in Air-Entrained and Non-Air-Entrained Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Range Water-Reducing Admixtures; Effect on the Air-Void System in Air-Entrained and Non-Air-Entrained Concrete

Author(s): Richard C. Mielenz and James H. Sprouse

Publication: Symposium Paper

Volume: 62

Issue:

Appears on pages(s): 167-192

Keywords: admixtures; air-entrained concretes; air entrainment; compressive strength; concrete durability; concretes; freeze-thaw durability; fresh concretes; hardened concretes; laboratories; plasticizers; tests; water content; water-reducing agents

DOI: 10.14359/17725

Date: 1/1/1979

Abstract:
Four commercial high-range water-reducing admixtures based on naphthlanene-sulfonic acid-formaldehyde condensation products and two commerical admixtures of this type based on melamine-sulfonic acid formaldehyde condensates were investigated to determine their effect on the air-void system in fresh and hardened concrete.