Fatigue Characteristics of Welded Wire Fabric

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fatigue Characteristics of Welded Wire Fabric

Author(s): N.M. Hawkins and L.W. Heaton

Publication: Symposium Paper

Volume: 41

Issue:

Appears on pages(s): 183-202

Keywords: bending; cracking (fracturing); deformations (reinforcing steels); fatigue (materials); fatigue tests; reinforcing; steels; static tests; stresses; welded wire fabric

DOI: 10.14359/17682

Date: 1/1/1974

Abstract:
Results are reported of tests to determine the factors dictating the short life fatigue characteristics in air of a square smooth welded wire fabric consisting of No. 2 wires at 6 inch (15 cm) centers.