Tests of Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests of Reinforced Concrete Beams

Author(s): Arthur N. Talbot

Publication: Symposium Paper

Volume: 52

Issue:

Appears on pages(s): 123-190

Keywords:

DOI: 10.14359/17627

Date: 1/1/1976

Abstract:
Reinforced concrete, concrete-steel, and armored concrete are terms given to a construction composed principally of concrete and having a small amount of metal so embeded as to take the prinicpal tensile stresses and perhaps the secondary tensile and shearing stresses developed.