Long-Term Freeze-Thaw Durability of Concrete in Catch Basins, Sidewalks and Pavement Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Long-Term Freeze-Thaw Durability of Concrete in Catch Basins, Sidewalks and Pavement Slabs

Author(s): J. Hode Keyser and M. Kushner

Publication: Symposium Paper

Volume: 47

Issue:

Appears on pages(s): 191-210

Keywords: age-strength relation; air entrainment; catch basins; compressive strength; concrete pavements; concrete slabs; concretes; deterioration; freeze-thaw durability; long-time study; sidewalks; tensile strength

DOI: 10.14359/17611

Date: 1/1/1975

Abstract:
The City of Montreal has approximatively 65,000 catch-basins, 1639 miles of concrete sidewalk and 979 miles of concrete pavement. The paper gives the history of their long term freeze-thaw durability.