Factors Affecting the Durability of Concrete Bridge Decks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Factors Affecting the Durability of Concrete Bridge Decks

Author(s): Roger E. Carrier and Philip D. Cady

Publication: Symposium Paper

Volume: 47

Issue:

Appears on pages(s): 121-168

Keywords: bridge decks; calcium chlorides; concrete pavements; concretes; corrosion; cover; cracking (fracturing); curing; deicers; deterioration; durability; freeze-thaw durability; highway bridges; mix proportioning; moisture; mortars (material)

DOI: 10.14359/17609

Date: 1/1/1975

Abstract:
A survey of 249 four-year old Pennsylvania bridge decks was conducted for two purposes: To determine the condition of the decks with regard to the extent and severity of their deterioration, and to provide insight into the relative importance of those factors, or combination of factors, which cause deterioration.