Tests on a Prestressed Micro-Concrete Model of a Three Cell Box Beam Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests on a Prestressed Micro-Concrete Model of a Three Cell Box Beam Bridge

Author(s): R.A. Swann

Publication: Symposium Paper

Volume: 24

Issue:

Appears on pages(s): 333-352

Keywords: box beams; bridges (structures); diaphragms (concrete); fabrication; live loads; loads (forces); micro-concrete; models; precast concrete; prestressed concrete; prestressing; research; shear properties; static loads; strength; stresses;structural analysis

DOI: 10.14359/17595

Date: 1/1/1970

Abstract:
The building and testing of a one-sixteenth scale microconcrete model of a typical interior span of a proposed six lane viaduct is described.