Ultimate Strength of Reinforced Cocnrete Beams in Combined Bending and Torsion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ultimate Strength of Reinforced Cocnrete Beams in Combined Bending and Torsion

Author(s): C.D. Goode and M.A. Helmy

Publication: Symposium Paper

Volume: 18

Issue:

Appears on pages(s): 357-378

Keywords:

DOI: 10.14359/17575

Date: 1/1/1968

Abstract:
Tests on 27 rectangular beams with transverse and longitudinal reinforcement are described. In many of these only one category of reinforcement had yielded when the maximum strength was reached. A general theory for the prediction of the ultimate strength in bending and torsion is proposed and compared with test results.