Stress-Strain Relationship for Reinforced Concrete in Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stress-Strain Relationship for Reinforced Concrete in Tension

Author(s): Domingo J. Carreira and Kuang-Han Chu

Publication: Journal Proceedings

Volume: 83

Issue: 1

Appears on pages(s): 21-28

Keywords: cracking (fracturing); extensibility; reinforced concrete; shrinkage; slippage; stress-strain relationships; tensile strength; tension; tension tests

DOI: 10.14359/1756

Date: 1/1/1986

Abstract:
A stress-strain relationship to represent the overall behavior of reinforced concrete in tension, which includes the combined effects of cracking and slippage at cracks along the reinforcement, is proposed. The serpentine curve previously used for the compression stress-strain relationship is also used in tension with parameters that are physically insignificant. These parameters can be determined experimentally from reinforced concrete prismatic specimens or estimated from proposed empirical relationships. The effects of the testing procedures, gage length, shrinkage, reinforcement, test specimen characteristics, cracking, and concrete strength and extensibility on the stress-strain diagrams for plain and reinforced concrete in tension are discussed.