Classification of Fasteners for Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Classification of Fasteners for Concrete

Author(s): Ben L. Bird

Publication: Symposium Paper

Volume: 22

Issue:

Appears on pages(s): 31-44

Keywords: anchoring; anchors; bolts; concrete blocks; concretes; costs; drilling; expansion bolts; fasteners; inserts; lag bolts; loads (forces); nails; precast concrete; screws; studs; toggle bolts

DOI: 10.14359/17552

Date: 1/1/1969

Abstract:
There are six general considerations for fasteners: (1) load level, weight held; (2) load condition-dead, variable, vibratory, shock; (3) base material; (4) atmospheric condition; (5) in-place cost and (6) simplicity of design.