Title: Repair of Concrete Bridge Pavements

Author(s): L. Kampf

Publication: Symposium Paper

Volume: 21

Issue:

Appears on pages(s): 53-66

Keywords:

DOI: 10.14359/17544

Date: 1/1/1968

Abstract:
The mechanism of concrete failure is discussed. Concrete in a bridge deck is subjected to stresses resulting from six dimensional changes.