Load-Deflection Characteristics of Perforated Reinforced Concrete Floor Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load-Deflection Characteristics of Perforated Reinforced Concrete Floor Slabs

Author(s): G.M. Sabnis and F. Roll

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 473-486

Keywords: building codes; columns (supports); concrete slabs; deflection; floors; loads (forces); reinforced concrete; standards; tests

DOI: 10.14359/17522

Date: 1/1/1974

Abstract:
The results of tests on approximately 50 perforated reinforced concrete slabs, with particular emphasis on their load-deflection behavior, are presented.