Some Experimental Studies of Time-Dependent Deflections of Noncomposite and Composite Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Some Experimental Studies of Time-Dependent Deflections of Noncomposite and Composite Reinforced Concrete Beams

Author(s): K.M. Kripanarayanan and D.E. Branson

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 409-420

Keywords: beams (supports); compressive strength; creep properties; deflection; loads (forces); reinforced concrete

DOI: 10.14359/17519

Date: 1/1/1974

Abstract:
Presented in this paper are the results of limited experimental studies concerning time-dependent deflections of composite and non-composite reinforced concrete beams. The experimental results are compared with appropriate analytical expressions and found to be satisfactory.