Calculation of Instantaneous Deflections for Continuous Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Calculation of Instantaneous Deflections for Continuous Reinforced Concrete Beams

Author(s): P.D. Zuraski, C.G. Salmon, and A. Fattah Shaikh

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 315-332

Keywords: bending moments; computation; continuous beams; cracking (fracturing); deflection; flexural strength; loads (forces); moments of inertia; reinforced concrete; standards; stiffness

DOI: 10.14359/17515

Date: 1/1/1974

Abstract:
Deflections of continuous concrete beams are computed by six different approximate procedures.