Short Term Deformation of Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Short Term Deformation of Reinforced Concrete Beams

Author(s): B. Johnston

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 225-248

Keywords: beams (supports); bending moments; computation; cracking (fracturing); deflection; deformation; flexural strength; moment-curvature relationship; reinforced concrete; stiffness; tensile strength

DOI: 10.14359/17511

Date: 1/1/1974

Abstract:
A simplified method of computing the moment-curvature relationships for beams subject to flexure is presented which enables the non-linear behaviour of concrete in compression and the stiffening effect of the tensile zone between cracks to be taken into account. A means of calculating deflections and rotations from the computed moment curvature is shown to be straightfoward in application and of acceptable accuracy.