A Computer Analysis of Deflection of Statically Indeterminate Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Computer Analysis of Deflection of Statically Indeterminate Concrete Structures

Author(s): R.G. Dysdale and M. Saeed Mirza

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 179-204

Keywords: axial loads; beams (supports); computer programs; continuous beams; creep properties; deflection; frames; modulus of elasticity; reinforced concrete; reinforcing steels; shrinkage; static loads; statically indeterminate structures; structural analysis

DOI: 10.14359/17509

Date: 1/1/1974

Abstract:
This paper discusses the ability of an analytical method to predict the behavior of statically indeterminate reinforced concrete frames and beams.