State-of-the-Art Report Deflection of Two Way Reinforced Concrete Floor Systems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: State-of-the-Art Report Deflection of Two Way Reinforced Concrete Floor Systems

Author(s): ACI Committee 435

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 55-82

Keywords: beams (supports); cracking (fracturing); creep properties; deflection; flat concrete plates; flat concrete slabs; flexural strength; floors; modulus of elasticity; reinforced concrete; reviews; structural analysis; two-way slabs

DOI: 10.14359/17506

Date: 1/1/1974

Abstract:
This state of the art paper summarizes practical methods for calculating the deflection of two-way slab systems, including flat slabs, flat plates, beam-supported slabs, and wall-supported slabs. A selected list of references is included.