Title: Transfer of Unbalanced Moment and Shear From Flat Plates to Columns

Author(s): N.M. Hawkins and W.G. Corley

Publication: Symposium Paper

Volume: 30

Issue:

Appears on pages(s): 147-176

Keywords: columns (supports); concrete slabs; connections; failure mechanisms; flat concrete plates; flexural strength; loads (forces); moments; reinforced concrete; research; shear properties; structural design; torsion

DOI: 10.14359/17494

Date: 1/1/1971

Abstract:
A refinement of current methods for calculating the strength of slab-column junctions carrying unbalanced moment and shear in flat plate concrete structures is described.




  