The Prediction and Control of Flexural Cracking in Reinforced Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Prediction and Control of Flexural Cracking in Reinforced Concrete Members

Author(s): A.W. Beeby

Publication: Symposium Paper

Volume: 30

Issue:

Appears on pages(s): 55-76

Keywords: conrete slabs; cracking (fracturing); crack width and spacing; failure mechanisms; flexural strength; loads (forces); reinforced conrete; research; stress concentration

DOI: 10.14359/17490

Date: 1/1/1971

Abstract:
The research work on cracking in reinforced concrete slabs carried out at the Cement and Concrete Association. . .A study of the problem is therefore made which leads to the formulation of a more general theory which is shown to agree well with the observed behavior.