Title: Distribution and Damping of Horizontal Force in Bridge Structures at Earthquake

Author(s): Fuijo Machida, Shusuke Miyazaki, Toshiyuki Kitta, Yasuo Maehara, Jiroh Iseki, and Ikuo Shimoda

Publication: Symposium Paper

Volume: 70

Issue:

Appears on pages(s): 1187-1224

Keywords: bridge bearings; bridge piers; bridges (structures); damping; dynamic structural analysis; earthquake resistant structures; earthquakes; joints (junctions); loads (forces); models; structural design; vibration

DOI: 10.14359/17457

Date: 1/1/1981

Abstract:
The combination of fixed bearings and movable bearings with damper stoppers offers one of bridge bearing systems for long span and multispan-continuous bridges.