Development of the Steel-Reinforced Elastomeric Expansion Joint Seal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of the Steel-Reinforced Elastomeric Expansion Joint Seal

Author(s): John A. Welch

Publication: Symposium Paper

Volume: 70

Issue:

Appears on pages(s): 1053-1066

Keywords: control joints; field tests; joints sealers; joints (junctions); reinforcing steels; research

DOI: 10.14359/17449

Date: 1/1/1981

Abstract:
This paper illustrates the development of reinforced elastomeric expansion joint seals. It outlines the laboratory procedures and simulated-service and field testing necessary to achiever a balance in design and materials to comply with engineering requirements. The paper also reveals the scope of studies - many performed at the request of government and consulting agencies - which determine recommendations for anchors, sealants, installartion methods, materials, and other peripheral elements. It further establishes the reliability of current sealing systems and indicates how current research and development projects can result in advanced systems for future applications.