Urethane Sealants for Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Urethane Sealants for Concrete Structures

Author(s): Robert M. Evans and R.B. Greene

Publication: Symposium Paper

Volume: 70

Issue:

Appears on pages(s): 983-996

Keywords: chemical analysis; durability; joint sealers; physical properties; specifications; structural design; structures; underwater structures; urethanes

DOI: 10.14359/17445

Date: 1/1/1981

Abstract:
The paper begins with a brief discussion of urethan chemistry as it relates to the properties of joint sealants. . .Urethanes are available in two component (on site mixing required) and one component forms. The chemistry and advantages of each type are discussed. . .Examples of urethane sealant use in vertical structures, horizontal structures and water immersed structures are given. Optimum and economical joint design for these are given.