Extruded Seals for Bridges and Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Extruded Seals for Bridges and Structures

Author(s): Guy S. Puccio

Publication: Symposium Paper

Volume: 70

Issue:

Appears on pages(s): 957-982

Keywords: bridges (structures); control joints; extrusions; installing; joint sealers; pavements; performance; physical properties; plastic, polymers and resins; specifications

DOI: 10.14359/17444

Date: 1/1/1981

Abstract:
Since 1960, many alternative materials have been available for sealing conctraction and expansion joints in pavements and numerous devices have been manufactured for sealing bridge expansion joint s. The extruded elastomeric seal is one such product. This paper discusses those parameters and attributes that make extruded seals a viable engineering material for expansion joints in bridges and structures.