Anchoring of Bearings by Friction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Anchoring of Bearings by Friction

Author(s): lngo Schrage

Publication: Symposium Paper

Volume: 70

Issue:

Appears on pages(s): 197-215

Keywords: anchorage (structural); bearings; friction; loads (forces); rubber; strains.

DOI: 10.14359/17410

Date: 1/1/1981

Abstract:
A review of slip resistance values is given for the interaction between several materials common in bearings for civil engineering. Friction between rubber and concrete is emphazised. Recent test results on bearing pads (plain rubber-bearings) and on specimens representing the outer layer of laminated bearings (reinforced rubber-bearings) are communicated. Those tests have been initiated in order to verify the assumption, that non-anchored rubber-bearings are appropriate to transfer short term tangential life loads without slip. Reinforced bearings follow some essentials of Coulomb's friction laws. As for friction coefficient vs. normal stress and vs. slip velocity rubber behaves unlike rigid solids. From the engineering point of view these statements are also good for bearing pads within the investigated range, though there are fundamental differences between those two kinds of bearing as far as response to lateral forces is concerned. There are only few national codes of practice for the "anchoring" of non-anchored rubber-bearings by the effects of friction. Among them the nowadays building regulations in Germany may serve as an approach to this aim. Nevertheless these regulations might become less restrict with regard to reinforced bearings on concrete, whereas frictional attachement of rubber to other materials should be handled with caution. Plain bearings need a new formulation of the slip criterion. Influences by the strain rate and by ambient temperature should be taken into account too.