The Influence of Porosity and Partial Drying on Properties of Polymer Impregnated Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Influence of Porosity and Partial Drying on Properties of Polymer Impregnated Mortar

Author(s): David G. Manning and Brian B. Hope

Publication: Symposium Paper

Volume: 40

Issue:

Appears on pages(s): 191-204

Keywords: compressive strength; cracking (fracturing); drying; high-early strength cements; humidity; impregnating; methyl methcrylate; mortars (material); polymer concrete; porosity; shirnkage; stress-strain relationships; styrene; tests

DOI: 10.14359/17390

Date: 1/1/1973

Abstract:
Three mortar mixes of widely differing porosities were impregnated with three vinyl monomers and methanol.