Title: A Study of Partially Impregnated Polymerized Concrete Specimens

Author(s): B. Sopler, A.E. Fiorato, and R. Lenschow

Publication: Symposium Paper

Volume: 40

Issue:

Appears on pages(s): 149-172

Keywords: compressive strength; concretes; creep properties; curing; deformaton; impregnating; methyl methacrylate; modulus of elasticity; polymer concrete; porosity; shrinkage; stress-strength relationships; tensile strength; tests; voids; water

DOI: 10.14359/17388

Date: 1/1/1973

Abstract:
An experimental program to study the preparation and properties of partially impregnated polymerized concrete specimens is described.