Some Observations on the Dynamic Sway Characteristics of Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Some Observations on the Dynamic Sway Characteristics of Concrete Structures

Author(s): A. P. Jeary and P.R. Sparks

Publication: Symposium Paper

Volume: 60

Issue:

Appears on pages(s): 155-180

Keywords: damping; dynamic characteristics; dynamic structural analysis; earthquakes; high-rise buildings; multistory buildings; reinforced concrete; stiffness; wind pressure

DOI: 10.14359/17375

Date: 1/1/1979

Abstract:
Since 1973, the Building Research Establishment has been making observations of the dynamic behavior of a number of concrete structures as part of a research programme investigating the response of structures to wind excitation. . .The paper describes the experimental technique used in the vibrator tests and discusses the results obtained and their implications.