Frequency Matching in Continuous Post-Tensioned Concrete Highway Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Frequency Matching in Continuous Post-Tensioned Concrete Highway Bridges

Author(s): T.I. Campbell, P.F. Csagoly, and A.C. Agarwal

Publication: Symposium Paper

Volume: 60

Issue:

Appears on pages(s): 139-154

Keywords: bridge decks; concrete slabs; continuous beams; damping capacity; dynamic loads; dynamic tests; highway bridges; impact; post-tensioning; structural analysis; vibrations

DOI: 10.14359/17374

Date: 1/1/1979

Abstract:
Results from dynamic load tests on a number of highway bridges of various types are presented.