The Modulus of Concrete and the Coefficient of Expansion of Concrete and Reinforced Concrete at Below Normal Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Modulus of Concrete and the Coefficient of Expansion of Concrete and Reinforced Concrete at Below Normal Temperatures

Author(s): Carl Berwanger

Publication: Symposium Paper

Volume: 25

Issue:

Appears on pages(s): 191-234

Keywords: age; bridge decks; bridges (structures); composite construction (concrete & steel); concrete slabs; concretes; dynamic modulus of elasticity; low temperature; modulus of elasicity; reinforced concrete; reinforcing steels; research; strain gages; strains

DOI: 10.14359/17337

Date: 1/1/1971

Abstract:
The dynamic modulus of the concrete and the coefficent of expansion of concrete and reinforced concrete slabs have been determined in the tests reported.