Compressive Strength of Concrete at Temperatures to 1600F

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compressive Strength of Concrete at Temperatures to 1600F

Author(s): M.S. Abrams

Publication: Symposium Paper

Volume: 25

Issue:

Appears on pages(s): 33-58

Keywords: aggregates; carbonate aggregates; compressive strength; concretes; expanded shale aggregates; fire resistance; high temperature tests; lightweight aggreagate concretes; ligh-weight aggregates; petrography; plain concrete; research; siliceous aggregates

DOI: 10.14359/17331

Date: 1/1/1971

Abstract:
Compressive strength tests were conducted on 3 x 6 in. (735 x 15 cm) cylindrical specimens heated for short duration to temperatures of 200 to 1600F (93 to 871C).