Title: Mass Concrete Practices in France

Author(s): Pierre Jacquin and J.F. Orth (Translated by Margaret Corbin)

Publication: Symposium Paper

Volume: 6

Issue:

Appears on pages(s): 103-126

Keywords:

DOI: 10.14359/17321

Date: 1/1/1963

Abstract:
Mass concrete practice in France is reviewed with special empahsis on heat of hydration and concrete composition. Durability and measurement of the workability of concrete are included along with a discussion of placing techniques.