Corps of Engineers Experience with Pozzolans

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Corps of Engineers Experience with Pozzolans

Author(s): William R. Waugh

Publication: Symposium Paper

Volume: 6

Issue:

Appears on pages(s): 89-102

Keywords:

DOI: 10.14359/17320

Date: 1/1/1963

Abstract:
Reports Corps of Engineers experience with the use of pozzolans in mass concrete, the investigation resulting in the present Corps specification for pozzolans. States that no serious problems resulted and that measurable reductions in water requirement was evident.